WebApr 1, 2015 · I use 5 tanks. First is for hot cleaner. This is 150 degrees and parts are in for 20 minutes. 2nd is for hot water rinse (to remove any oil and hold compound). this is kept just under boil. Parts are in for 5 minutes. 3rd for hot salts. This is at 285 degrees and parts are in for 30 minutes. 4th for hot water rinse with sat removing solution ... WebNov 16, 2024 · Hot Bluing. 1. Scrub the piece in cold water. Submerge the piece in cold …
Gun Bluing 101 – How to Blue a Gun - Makers Legacy
WebHot bluing refers to one of these two techniques. Hot bluing can be done in a variety of ways. Hot bluing is the latest industry norm for gun bluing, as it and rust bluing provide the best long-term rust resistance and cosmetic protection for exposed gunmetal. To begin the basic browning process, dissolve regular table salt in distilled water. WebAug 8, 2011 · Tips & Tricks . Caustic (hot) blue. Thread ... . Caustic (hot) blue. Thread … jax build pro
"Low Temp" Hot Black Oxide? - finishing.com
WebNov 26, 2010 · The Superposed for most of it's life used 2 different bluing processes. Slow rust bluing on the barrels and Belgian bluing on the frame and associated parts. Later years may well have changed the bluing method on the frame but the barrels and ribs were/are soft soldered which won't take hot caustic bluing without coming apart. Parris Web2007. Hi David, hot bluing is the most simplest method to blue your gun.here is how you do...1.clean and remove all pits and rust using emery sheet 400,followed by emery 800. 2.if possible buffing can save lot of time and energy. 3.make sure you have no finger prints or dust. 4.use a news paper to hold the parts and wipe clean. 5.mix 1kg of ... Webhttp://americangunsmith.com/youtube Gene Shuey shows you how to refinish your … low roll tires 196/65r15 discount tires